Superalliages à base Nickel élaborés par fabrication additive fil à haut taux de dépôt avec écrouissage inter-passes : Influence des cycles thermiques sur les microstructures et les performances mécaniques. // Nickel-Based Superalloys Produced by High-Dep
- Electronique
Fabrication additive, Superalliage à base Nickel, EBSD, Microstructure, Traitement thermique, Comportement
Additive manufacturing , Nickel-based superalloys, EBSD , Microstructure, Heat treatment, Mechanical behavior
Additive manufacturing , Nickel-based superalloys, EBSD , Microstructure, Heat treatment, Mechanical behavior
Description du sujet
Le procédé de fabrication additive par arc-fil (WAAM) constitue une alternative prometteuse aux procédés conventionnels pour la réalisation de composants de grande dimension, offrant un excellent rendement matière, des taux de dépôt élevés synonyme de gains de productivité, et des performances mécaniques comparables, voire supérieures. Toutefois, le WAAM reste limité par des verrous majeurs, e.g. hétérogénéité microstructurale, phases secondaires fragiles, contraintes résiduelles. Le profil thermique au cours du dépôt pilote l'évolution microstructurale et conditionne les propriétés du matériau. Or, dans les procédés WAAM conventionnels, l'apport thermique est couplé au taux de dépôt, ce qui limite la capacité à ajuster indépendamment les cycles thermiques et à maîtriser finement les microstructures et les performances. Un procédé hybride innovant de type WAAM MIG à fil froid (CW-MIG WAAM), développé à l'Université de Cranfield, permet de découpler l'apport thermique du débit de matériau, offrant un contrôle fin des cycles thermiques. Combiné à des stratégies de déformation plastique à froid et étendu dans ce projet à la déformation à chaud en cours de dépôt, ce procédé ouvre de nouvelles perspectives de contrôle microstructural. Cette thèse vise à développer une compréhension des liens entre cycles thermiques, évolutions microstructurales et propriétés mécaniques, afin d'évaluer le potentiel du procédé CW-MIG WAAM à haut taux de dépôt, combiné à la déformation à chaud en cours de dépôt, pour la production de composants en superalliages à base nickel à hautes performances.
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
Additive manufacturing by wire arc (WAAM) is a promising alternative to conventional processes for the production of large-scale components, offering high material efficiency, high deposition rates associated with productivity gains, and mechanical properties that are comparable or even superior. However, WAAM remains limited by major challenges, e.g. microstructural heterogeneity, brittle secondary phases, and residual stresses. The thermal profile during deposition governs microstructural evolution and therefore determines the material properties. In conventional WAAM processes, heat input is coupled with deposition rate, which limits the ability to independently tailor thermal cycles and to finely control microstructures and properties. An innovative hybrid process based on cold-wire MIG WAAM (CW-MIG WAAM), developed at Cranfield University, enables the decoupling of heat input from material feed rate, providing precise control of thermal cycles. When combined with cold plastic deformation strategies and extended in this project to in-situ hot deformation during deposition, this process opens new perspectives for microstructural control. This PhD project aims to develop an understanding of the relationships between thermal cycles, microstructural evolution, and mechanical properties, in order to assess the potential of high-deposition-rate CW-MIG WAAM combined with in-process hot deformation for the production of high-performance nickel-based superalloy components.
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
Début de la thèse : 01/10/2026
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
Additive manufacturing by wire arc (WAAM) is a promising alternative to conventional processes for the production of large-scale components, offering high material efficiency, high deposition rates associated with productivity gains, and mechanical properties that are comparable or even superior. However, WAAM remains limited by major challenges, e.g. microstructural heterogeneity, brittle secondary phases, and residual stresses. The thermal profile during deposition governs microstructural evolution and therefore determines the material properties. In conventional WAAM processes, heat input is coupled with deposition rate, which limits the ability to independently tailor thermal cycles and to finely control microstructures and properties. An innovative hybrid process based on cold-wire MIG WAAM (CW-MIG WAAM), developed at Cranfield University, enables the decoupling of heat input from material feed rate, providing precise control of thermal cycles. When combined with cold plastic deformation strategies and extended in this project to in-situ hot deformation during deposition, this process opens new perspectives for microstructural control. This PhD project aims to develop an understanding of the relationships between thermal cycles, microstructural evolution, and mechanical properties, in order to assess the potential of high-deposition-rate CW-MIG WAAM combined with in-process hot deformation for the production of high-performance nickel-based superalloy components.
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
------------------------------------------------------------------------------------------------------------------------------------------------------------------------
Début de la thèse : 01/10/2026
Nature du financement
Contrat doctoral
Précisions sur le financement
Concours pour un contrat doctoral
Présentation établissement et labo d'accueil
Université de Technologie de Compiègne
Etablissement délivrant le doctorat
Université de Technologie de Compiègne
Ecole doctorale
71 Sciences pour l'ingénieur
Profil du candidat
Le (la) candidat(e) devra :
- Être titulaire d'une formation Bac+5 (Master ou équivalent) en sciences des matériaux ou en génie mécanique.
- Posséder des connaissances solides en métallurgie, procédés de fabrication additive et comportement mécanique des matériaux.
- Avoir de bonnes compétences dans les techniques de caractérisation des matériaux (MEB, EBSD, MET).
- Faire preuve d'autonomie, de rigueur scientifique et d'esprit critique dans l'analyse et l'interprétation des résultats expérimentaux.
- Avoir la capacité de travailler au sein d'équipes pluridisciplinaires.
- Être motivé(e) par la recherche.
The candidate should: - Hold a Master's degree (or equivalent) in Materials Science or Mechanical Engineering. - Have strong knowledge in metallurgy, additive manufacturing processes, and the mechanical behavior of materials. - Possess good skills in material characterization techniques (SEM, EBSD, TEM). - Demonstrate autonomy, scientific rigor, and critical thinking in the analysis and interpretation of experimental results. - Be able to work effectively within multidisciplinary teams. - Be motivated by research.
The candidate should: - Hold a Master's degree (or equivalent) in Materials Science or Mechanical Engineering. - Have strong knowledge in metallurgy, additive manufacturing processes, and the mechanical behavior of materials. - Possess good skills in material characterization techniques (SEM, EBSD, TEM). - Demonstrate autonomy, scientific rigor, and critical thinking in the analysis and interpretation of experimental results. - Be able to work effectively within multidisciplinary teams. - Be motivated by research.
15/05/2026
Postuler
Fermer
Vous avez déjà un compte ?
Nouvel utilisateur ?
Vous souhaitez recevoir nos infolettres ?
Découvrez nos adhérents
Laboratoire National de Métrologie et d'Essais - LNE
Ifremer
Institut Sup'biotech de Paris
SUEZ
Servier
ADEME
Aérocentre, Pôle d'excellence régional
ONERA - The French Aerospace Lab
TotalEnergies
Généthon
Groupe AFNOR - Association française de normalisation
Nokia Bell Labs France
ASNR - Autorité de sûreté nucléaire et de radioprotection - Siège
Tecknowmetrix
ANRT
Nantes Université
Medicen Paris Region